等级 | 厂家 | 型号 | 特性 | 用途 |
---|---|---|---|---|
阻燃级 | 科思创 ® Covestro | FR1514 | (PC + ABS) - 共混; 高耐热性; UL识别94 V-0,1.5 mm | 适合作为带电部件的支撑材料 |
阻燃级 | 科思创 ® Covestro | FR3040 | UL识别94 V-0在0.75 mm及以上,V-1在0.6 mm,120温度= 108℃; HDT / A> = 85°C; | 薄壁应用; 小壁厚的非常好的燃烧性能 |
阻燃级 | 科思创 ® Covestro | M303FR | 中粘度,阻燃性,维卡/ B 120温度= 115°C; | 电气和电子设备; 根据GMP制造 |
阻燃级 | 科思创 ® Covestro | FR3000 | 抗紫外线性能良好 良好的流动性 阻燃性 | 薄壁应用; 小壁厚的非常好的燃烧性能 |
阻燃级 | 科思创 ® Covestro | FR3008 | 抗紫外线性能良好 耐化学性良好 耐水解性 阻燃性 | 汽车业、电气和电子行业 |
阻燃级 | 科思创 ® Covestro | FR3010 | 120温度= 110°C; 增加耐热性; UL识别94 V-0,1.5 mm; 灼热丝温度(GWFI):960℃,2.0mm; 提高耐化学性和应力开裂行为; | 适合作为带电部件的支撑材料 |
Rheological properties | Value | Unit | Test Standard |
Melt volume-flow rate, MVR | 19 | cm3/10min | ISO 1133 |
Temperature | 500 | °F | ISO 1133 |
Load | 11 | lb | ISO 1133 |
Mechanical properties | Value | Unit | Test Standard |
Tensile modulus | 348091 | psi | ISO 527-1/-2 |
Yield stress | 9140 | psi | ISO 527-1/-2 |
Yield strain | 5 | % | ISO 527-1/-2 |
Thermal properties | Value | Unit | Test Standard |
Temp. of deflection under load, 1.80 MPa | 237 | °F | ISO 75-1/-2 |
Temp. of deflection under load, 0.45 MPa | 259 | °F | ISO 75-1/-2 |
Vicat softening temperature, 50°C/h 50N | 273 | °F | ISO 306 |
Coeff. of linear therm. expansion, parallel | 68 | E-6/K | ISO 11359-1/-2 |
Coeff. of linear therm. expansion, normal | 68 | E-6/K | ISO 11359-1/-2 |
Burning behavior at 1.5 mm nominal thickness | V-0 | class | IEC 60695-11-10 |
Thickness tested (1.5) | 0.1 | in | IEC 60695-11-10 |
Burning behavior 5V at thickness h | 5VB | class | IEC 60695-11-20 |
Thickness tested | 0.1 | in | IEC 60695-11-20 |
Oxygen index | 30 | % | ISO 4589-1/-2 |
Electrical properties | Value | Unit | Test Standard |
Relative permittivity, 100Hz | 3.2 | - | IEC 62631-2-1 |
Relative permittivity, 1MHz | 3.1 | - | IEC 62631-2-1 |
Dissipation factor, 100Hz | 20 | E-4 | IEC 62631-2-1 |
Dissipation factor, 1MHz | 85 | E-4 | IEC 62631-2-1 |
Volume resistivity | >1E13 | Ohm*m | IEC 62631-3-1 |
Surface resistivity | >1E15 | Ohm | IEC 62631-3-2 |
Electric strength | 889 | kV/in | IEC 60243-1 |
Comparative tracking index | 350 | - | IEC 60112 |
Other properties | Value | Unit | Test Standard |
Water absorption | 0.5 | % | Sim. to ISO 62 |
Humidity absorption | 0.2 | % | Sim. to ISO 62 |
Density | 1190 | kg/m3 | ISO 1183 |
Test specimen production | Value | Unit | Test Standard |
Injection molding, melt temperature | 500 | °F | ISO 294 |
Injection molding, mold temperature | 176 | °F | ISO 294 |
Injection molding, injection velocity | 9.45 | in/s | ISO 294 |