Processing/Physical Characteristics
|
Value
|
Unit
|
Test Standard
|
ISO Data
|
Melt volume-flow rate, MVR
|
3.4
|
cm3/10min
|
ISO 1133
|
Temperature
|
190
|
°C
|
-
|
Load
|
2.16
|
kg
|
-
|
Mechanical properties
|
Value
|
Unit
|
Test Standard
|
ISO Data
|
Tensile Modulus
|
2750
|
MPa
|
ISO 527
|
Yield stress
|
62
|
MPa
|
ISO 527
|
Yield strain
|
10
|
%
|
ISO 527
|
Strain at break
|
35
|
%
|
ISO 527
|
Flexural modulus, 23°C
|
2450
|
MPa
|
ISO 178
|
Flexural strength
|
88
|
MPa
|
ISO 178
|
Charpy notched impact strength, +23°C
|
8
|
kJ/m2
|
ISO 179/1eA
|
Thermal properties
|
Value
|
Unit
|
Test Standard
|
ISO Data
|
Melting temperature, 10°C/min
|
165
|
°C
|
ISO 11357-1/-3
|
Temp. of deflection under load, 1.80 MPa
|
100
|
°C
|
ISO 75-1/-2
|
Coeff. of linear therm. expansion, parallel
|
110
|
E-6/K
|
ISO 11359-1/-2
|
Coeff. of linear therm. expansion, normal
|
110
|
E-6/K
|
ISO 11359-1/-2
|
Burning behav. at thickness h
|
HB
|
class
|
IEC 60695-11-10
|
Thickness tested
|
0.8
|
mm
|
-
|
Yellow Card available
|
yes
|
-
|
-
|
Other properties
|
Value
|
Unit
|
Test Standard
|
Humidity absorption
|
0.22
|
%
|
Sim. to ISO 62
|
Density
|
1410
|
kg/m3
|
ISO 1183
|
Processing Recommendation Injection Molding
|
Value
|
Unit
|
Test Standard
|
Pre-drying - Temperature
|
80
|
°C
|
-
|
Pre-drying - Time
|
3 - 4
|
h
|
-
|
Mold temperature
|
60 - 80
|
°C
|
-
|
Zone 1
|
170
|
°C
|
-
|
Zone 2
|
180
|
°C
|
-
|
Zone 3
|
190
|
°C
|
-
|
Nozzle temperature
|
180 - 210
|
°C
|
-
|
Screw speed
|
80 - 120
|
rpm
|
-
|
Injection pressure
|
50 - 100
|
MPa
|
-
|
Characteristics
Processing
Injection Molding
Features
Copolymer
Certifications
Drinking water contact
Applications
Automotive, Electrical and Electronical, General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa